General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.1 g/cm³ Show Supplier Material materials with Densidad of 8.1 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 0.05 % Show Supplier Material materials with Carbono of 0.05 % | max. | |
Hierro | balance | ||
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | max. | |
Níquel | 35 - 37 % Show Supplier Material materials with Níquel of 35 - 37 % | ||
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % | max. |