Medidas
Property | Value |
---|---|
Dimensions | <p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p> |
Mecánica
Property | Value | Comment |
---|---|---|
Límite elástico | 160 MPa Show Supplier Material materials with Límite elástico of 160 MPa | RP02 |
Resistencia a la tracción | 160 - 220 MPa Show Supplier Material materials with Resistencia a la tracción of 160 - 220 MPa |
Aplicaciones térmicas
Property | Value |
---|
Eléctrico
Property | Value | Comment |
---|---|---|
Potencial de corrosión | -690 mV Show Supplier Material materials with Potencial de corrosión of -690 mV | |
Resistividad eléctrica | 3.4e-08 - 4.3e-08 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.4e-08 - 4.3e-08 Ω·m | Changes depending on temper |
Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Circonio | 0 - 0.1 % Show Supplier Material materials with Circonio of 0 - 0.1 % |
Cobre | 0.4 - 0.7 % Show Supplier Material materials with Cobre of 0.4 - 0.7 % |
Hierro | 0.1 - 0.5 % Show Supplier Material materials with Hierro of 0.1 - 0.5 % |
Manganeso | 1.2 - 1.6 % Show Supplier Material materials with Manganeso of 1.2 - 1.6 % |
Silicona | 0.4 - 0.8 % Show Supplier Material materials with Silicona of 0.4 - 0.8 % |
Titanio | 0.1 - 0.2 % Show Supplier Material materials with Titanio of 0.1 - 0.2 % |
Zinc | 0 - 0.1 % Show Supplier Material materials with Zinc of 0 - 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers | |
Processing history | Temper: H24 |