Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Aluminium Alloy Braze clad - Vacuum FA 6693
Los datos sobre este material han sido proporcionados por Gränges.
All categories
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Coeficiente de dilatación térmica | 2.36e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | for 20-100°C |
Temperatura de fusión | 556 °C Show Supplier Material materials with Temperatura de fusión of 556 °C | Mean |
Chemical properties
Property | Value |
---|---|
Zinc | 0.2 % Show Supplier Material materials with Zinc of 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.