General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Densidad | 2.413 - 2.667 g/cm³ Show Supplier Material materials with Densidad of 2.413 - 2.667 g/cm³ | ||
Densidad relativa | 99.8 [-] Show Supplier Material materials with Densidad relativa of 99.8 [-] | min. | Optical density determination at test specimen by light microscopy | |
Mean Roughness | 8 μm Show Supplier Material materials with Mean Roughness of 8 μm | DIN EN ISO 16610-21 | |
Mean Roughness Depth | 50 μm Show Supplier Material materials with Mean Roughness Depth of 50 μm | DIN EN ISO 16610-21 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongación | 1.5 % Show Supplier Material materials with Elongación of 1.5 % | min. | |
Límite elástico | 115 MPa Show Supplier Material materials with Límite elástico of 115 MPa | min., RP02 | |
Módulo elástico | 90 GPa Show Supplier Material materials with Módulo elástico of 90 GPa | min. | |
Resistencia a la tracción | 200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | DIN EN ISO 6892-1 Method B | min. |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Coeficiente de dilatación térmica | 1.46e-05 - 1.56e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.46e-05 - 1.56e-05 1/K | for 20-100°C |
1.55e-05 - 1.65e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.55e-05 - 1.65e-05 1/K | for 20-200°C | |
1.63e-05 - 1.73e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.63e-05 - 1.73e-05 1/K | for 20-300°C |
Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Silicona | 34 - 36 % Show Supplier Material materials with Silicona of 34 - 36 % |
Technological properties
Property | ||
---|---|---|
Application areas | The material is used in a wide range of industries such as linear technology, optical industry and aerospace. Typical applications include housings, moving components and other lightweight applications. | |
Other | The properties in this material data sheet reflect minimum values that are achieved when printing S220 powder on an industrial Additive Manufacturing (AM) machine. The machine used is a Concept Laser M2, Laser Powder Bed Fusion category. |