General
Property | Value | Comment |
---|---|---|
Densidad | 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.22 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 95.0 [-] Show Supplier Material materials with Dureza Shore A of 95.0 [-] | ASTM D2240 |
Elongación | 600.0 % Show Supplier Material materials with Elongación of 600.0 % | ASTM D412 |
Resistencia a desgarros | 180.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 180.0 kN/m | ASTM D624 |
Resistencia a la tracción | 60.0 MPa Show Supplier Material materials with Resistencia a la tracción of 60.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods. |