General
Property | Value | Comment |
---|---|---|
Densidad | 1.16 g/cm³ Show Supplier Material materials with Densidad of 1.16 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 55.0 [-] Show Supplier Material materials with Dureza Shore D of 55.0 [-] | ASTM D2240 |
Elongación | 430.0 % Show Supplier Material materials with Elongación of 430.0 % | ASTM D412 |
Resistencia a desgarros | 150.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 150.0 kN/m | ASTM D624 |
Resistencia a la tracción | 47.0 MPa Show Supplier Material materials with Resistencia a la tracción of 47.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Apparel Applications And Outdoor Applications. |