General
Property | Value | Comment |
---|---|---|
Densidad | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 81.0 [-] Show Supplier Material materials with Dureza Shore D of 81.0 [-] | ASTM D2240 |
Elongación | 40.0 % Show Supplier Material materials with Elongación of 40.0 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 108 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 108 J/m | ASTM D256 |
Módulo de flexión | 1.85 GPa Show Supplier Material materials with Módulo de flexión of 1.85 GPa | ASTM D790 |
Módulo elástico | 1.57 GPa Show Supplier Material materials with Módulo elástico of 1.57 GPa | ASTM D638 |
Resistencia a la flexión | 108.0 MPa Show Supplier Material materials with Resistencia a la flexión of 108.0 MPa | ASTM D790 |
Resistencia a la tracción | 83.0 MPa Show Supplier Material materials with Resistencia a la tracción of 83.0 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 105.0 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 105.0 °C | 0.45 MPa | ASTM D648 |
Temperatura de reblandecimiento Vicat | 112.0 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 112.0 °C | ASTM D1525 |
Technological properties
Property | ||
---|---|---|
Application areas | Electronics, Automotive, Power Tools, Oil-Water Separator, Optics Products. |