General
Property | Value | Comment |
---|---|---|
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 80.0 [-] Show Supplier Material materials with Dureza Shore D of 80.0 [-] | ASTM D2240 |
Elongación | 193.0 % Show Supplier Material materials with Elongación of 193.0 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 108 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 108 J/m | ASTM D256 |
Módulo de flexión | 1.63 GPa Show Supplier Material materials with Módulo de flexión of 1.63 GPa | ASTM D790 |
Módulo elástico | 1.28 GPa Show Supplier Material materials with Módulo elástico of 1.28 GPa | ASTM D638 |
Resistencia a la flexión | 88.0 MPa Show Supplier Material materials with Resistencia a la flexión of 88.0 MPa | ASTM D790 |
Resistencia a la tracción | 68.0 MPa Show Supplier Material materials with Resistencia a la tracción of 68.0 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 65.0 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 65.0 °C | 0.45 MPa | ASTM D648 |
Temperatura de reblandecimiento Vicat | 77.0 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 77.0 °C | ASTM D1525 |
Technological properties
Property | ||
---|---|---|
Application areas | Electronics, Automotive, Power Tools, Oil-Water Separator, Optics Products. |