General
Property | Value | Comment |
---|---|---|
Densidad | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 76.0 [-] Show Supplier Material materials with Dureza Shore D of 76.0 [-] | ASTM D2240 |
Elongación | 150.0 % Show Supplier Material materials with Elongación of 150.0 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 1060 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 1060 J/m | ASTM D256 |
Módulo de flexión | 1.37 GPa Show Supplier Material materials with Módulo de flexión of 1.37 GPa | ASTM D790 |
Módulo elástico | 1.08 GPa Show Supplier Material materials with Módulo elástico of 1.08 GPa | ASTM D638 |
Resistencia a la flexión | 74.0 MPa Show Supplier Material materials with Resistencia a la flexión of 74.0 MPa | ASTM D790 |
Resistencia a la tracción | 60.0 MPa Show Supplier Material materials with Resistencia a la tracción of 60.0 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 90.0 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 90.0 °C | 0.45 MPa | ASTM D648 |
Temperatura de reblandecimiento Vicat | 98.0 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 98.0 °C | ASTM D1525 |
Technological properties
Property | ||
---|---|---|
Application areas | Electronics, Automotive, Power Tools, Oil-Water Separator, Optics Products. |