General
Property | Value | Comment |
---|---|---|
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 78.0 [-] Show Supplier Material materials with Dureza Shore D of 78.0 [-] | ASTM D2240 |
Elongación | 92.0 % Show Supplier Material materials with Elongación of 92.0 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 646 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 646 J/m | ASTM D256 |
Módulo de flexión | 1.58 GPa Show Supplier Material materials with Módulo de flexión of 1.58 GPa | ASTM D790 |
Módulo elástico | 1.35 GPa Show Supplier Material materials with Módulo elástico of 1.35 GPa | ASTM D638 |
Resistencia a la flexión | 91.0 MPa Show Supplier Material materials with Resistencia a la flexión of 91.0 MPa | ASTM D790 |
Resistencia a la tracción | 67.0 MPa Show Supplier Material materials with Resistencia a la tracción of 67.0 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 110.0 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 110.0 °C | 0.45 MPa | ASTM D648 |
Temperatura de reblandecimiento Vicat | 129.0 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 129.0 °C | ASTM D1525 |
Technological properties
Property | ||
---|---|---|
Application areas | Electronics, Automotive, Power Tools, Oil-Water Separator, Optics Products. |