General
Property | Value | Comment |
---|---|---|
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 91.0 [-] Show Supplier Material materials with Dureza Shore A of 91.0 [-] | ASTM D2240 | |
Elongación | 450.0 % Show Supplier Material materials with Elongación of 450.0 % | ASTM D412 | |
Resistencia a desgarros | 120.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 120.0 kN/m | ASTM D624 | |
Resistencia a la tracción | 56.0 MPa Show Supplier Material materials with Resistencia a la tracción of 56.0 MPa | ASTM D638 | |
Set de compresión | 23 °C | 20 [-] Show Supplier Material materials with Set de compresión of 20 [-] | ASTM D395, for 22hrs |
70 °C | 28 [-] Show Supplier Material materials with Set de compresión of 28 [-] | ASTM D395, for 22hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods. |