General
Property | Value | Comment |
---|---|---|
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 90.0 [-] Show Supplier Material materials with Dureza Shore A of 90.0 [-] | ASTM D2240 | |
Elongación | 580.0 % Show Supplier Material materials with Elongación of 580.0 % | ASTM D412 | |
Resistencia a desgarros | 130.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 130.0 kN/m | ASTM D624 | |
Resistencia a la tracción | 30.0 MPa Show Supplier Material materials with Resistencia a la tracción of 30.0 MPa | ASTM D638 | |
Set de compresión | 100 °C | 33 [-] Show Supplier Material materials with Set de compresión of 33 [-] | ASTM D395, for 22hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods. |