General
Property | Value | Comment |
---|---|---|
Densidad | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 90.0 [-] Show Supplier Material materials with Dureza Shore A of 90.0 [-] | ASTM D2240 |
Elongación | 550.0 % Show Supplier Material materials with Elongación of 550.0 % | ASTM D412 |
Resistencia a desgarros | 120.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 120.0 kN/m | ASTM D624 |
Resistencia a la tracción | 54.0 MPa Show Supplier Material materials with Resistencia a la tracción of 54.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Apparel Applications And Outdoor Applications. |