Property | Value | Comment |
---|---|---|
Densidad | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 85.0 [-] Show Supplier Material materials with Dureza Shore A of 85.0 [-] | ASTM D2240 |
Elongación | 400.0 % Show Supplier Material materials with Elongación of 400.0 % | ASTM D412 |
Resistencia a desgarros | 115.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 115.0 kN/m | ASTM D624 |
Resistencia a la tracción | 43.0 MPa Show Supplier Material materials with Resistencia a la tracción of 43.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Protective Films and Smart Wearable Devices |