General
Property | Value | Comment |
---|---|---|
Densidad | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 85.0 [-] Show Supplier Material materials with Dureza Shore A of 85.0 [-] | ASTM D2240 |
Elongación | 570.0 % Show Supplier Material materials with Elongación of 570.0 % | ASTM D412 |
Resistencia a desgarros | 130.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 130.0 kN/m | ASTM D624 |
Resistencia a la tracción | 29.0 MPa Show Supplier Material materials with Resistencia a la tracción of 29.0 MPa | ASTM D412 |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL94 V0 (2mm) |
Technological properties
Property | ||
---|---|---|
Application areas | Building/Construction, Mining, Wire and Cables |