General
Property | Value | Comment |
---|---|---|
Densidad | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 95.0 [-] Show Supplier Material materials with Dureza Shore A of 95.0 [-] | ASTM D2240 |
Elongación | 438.0 % Show Supplier Material materials with Elongación of 438.0 % | ASTM D412 |
Módulo de flexión | 0.096 GPa Show Supplier Material materials with Módulo de flexión of 0.096 GPa | ASTM D790 |
Resistencia a desgarros | 190.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 190.0 kN/m | ASTM D624 |
Resistencia a la tracción | 51.0 MPa Show Supplier Material materials with Resistencia a la tracción of 51.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Tubing and Medical Disposable Applications. | |
Certifications | Bio-compatibility according to USP class VI |