General
Property | Value | Comment |
---|---|---|
Densidad | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 76.0 [-] Show Supplier Material materials with Dureza Shore D of 76.0 [-] | ASTM D2240 |
Elongación | 150.0 % Show Supplier Material materials with Elongación of 150.0 % | ASTM D412 |
Módulo de flexión | 1.37 GPa Show Supplier Material materials with Módulo de flexión of 1.37 GPa | ASTM D790 |
Resistencia a la tracción | 60.0 MPa Show Supplier Material materials with Resistencia a la tracción of 60.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Tubing and Medical Disposable Applications. | |
Certifications | Bio-compatibility according to USP class VI |