General
Property | Value |
---|---|
Densidad | 1.57 g/cm³ Show Supplier Material materials with Densidad of 1.57 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 2.0 % Show Supplier Material materials with Elongación of 2.0 % | |
Impact strength, Izod notched, ASTM | 400 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 400 J/m | ASTM D256 |
Módulo de flexión | 13.739 GPa Show Supplier Material materials with Módulo de flexión of 13.739 GPa | |
Resistencia a la flexión | 344.0 MPa Show Supplier Material materials with Resistencia a la flexión of 344.0 MPa | |
Resistencia a la tracción | 216.0 MPa Show Supplier Material materials with Resistencia a la tracción of 216.0 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Parts, Sports Equipment |