General
Property | Value |
---|---|
Densidad | 1.7 g/cm³ Show Supplier Material materials with Densidad of 1.7 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 1.8 % Show Supplier Material materials with Elongación of 1.8 % | |
Impact strength, Izod notched, ASTM | 370 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 370 J/m | ASTM D256 |
Módulo de flexión | 19.627 GPa Show Supplier Material materials with Módulo de flexión of 19.627 GPa | |
Resistencia a la flexión | 393.0 MPa Show Supplier Material materials with Resistencia a la flexión of 393.0 MPa | |
Resistencia a la tracción | 255.0 MPa Show Supplier Material materials with Resistencia a la tracción of 255.0 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Parts, Sports Equipment |