General
Property | Value |
---|---|
Densidad | 1.6 g/cm³ Show Supplier Material materials with Densidad of 1.6 g/cm³ |
Mecánica
Property | Value |
---|---|
Impact strength, Izod notched, ASTM | 394 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 394 J/m |
Módulo de flexión | 12.3 GPa Show Supplier Material materials with Módulo de flexión of 12.3 GPa |
Resistencia a la flexión | 315.0 MPa Show Supplier Material materials with Resistencia a la flexión of 315.0 MPa |
Resistencia a la tracción | 197.0 MPa Show Supplier Material materials with Resistencia a la tracción of 197.0 MPa |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 90.0 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 90.0 °C | 1.8 MPa | ASTM D648 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Automotive and Hand Tools. | |
Fillers | 50% Long Glass Fiber |