General
Property | Value |
---|---|
Densidad | 1.7 g/cm³ Show Supplier Material materials with Densidad of 1.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Impact strength, Izod notched, ASTM | -20 °C | 390 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 390 J/m |
23 °C | 490 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 490 J/m | |
Módulo de flexión | 17.69 GPa Show Supplier Material materials with Módulo de flexión of 17.69 GPa | |
Resistencia a la flexión | 365.0 MPa Show Supplier Material materials with Resistencia a la flexión of 365.0 MPa | |
Resistencia a la tracción | 225.0 MPa Show Supplier Material materials with Resistencia a la tracción of 225.0 MPa |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 220.0 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220.0 °C | 1.8 MPa | ASTM D648 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Car Industry, Frame in the engine bay, Seat frame, Dashboard frame, Frame of Battery base, Door panel, Pedals, Fender apron, Frame of spare tire. Electronics, High precision plug-in/element, Structure parts of the printer, Frame of the 3C products, Structure parts. Petrochemical, Corrosion and abrasion resistance parts, Grille platform, Parts of filtration facility, Reactor parts. Others, Seat frame of bicycle, Snowboard, Structure parts of the exercise gear and pedals, Toe of Safety boot, Safety helmet. | |
Fillers | 60% Glass Fiber |