General
Property | Value | Comment |
---|---|---|
Densidad | 1.16 g/cm³ Show Supplier Material materials with Densidad of 1.16 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Impact strength, Izod notched, ASTM | 215.2 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 215.2 J/m | ASTM D256 |
Límite elástico | 43.5 MPa Show Supplier Material materials with Límite elástico of 43.5 MPa | ASTM D638 |
Módulo de flexión | 1.96 GPa Show Supplier Material materials with Módulo de flexión of 1.96 GPa | ASTM D790 |
Resistencia a la flexión | 70.0 MPa Show Supplier Material materials with Resistencia a la flexión of 70.0 MPa | ASTM D790 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 79.0 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 79.0 °C | 1.8 MPa | ASTM D648 | ||
Temperatura de reblandecimiento Vicat | 95.0 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 95.0 °C | ASTM D1525, 1kg load | |||
Inflamabilidad | UL94 V0 (2.5mm) |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 45.0 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 45.0 g/10min | ASTM D1238, 220°C,10kg/cm2 |
Technological properties
Property | ||
---|---|---|
Application areas | Telephone housing, Tv housing |