General
Property | Value | Comment |
---|---|---|
Densidad | 1.1 g/cm³ Show Supplier Material materials with Densidad of 1.1 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Hardness, Rockwell R | 113.0 [-] Show Supplier Material materials with Hardness, Rockwell R of 113.0 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 98 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 98 J/m | ASTM D256 |
Límite elástico | 52.0 MPa Show Supplier Material materials with Límite elástico of 52.0 MPa | ASTM D638 |
Módulo de flexión | 2.31 GPa Show Supplier Material materials with Módulo de flexión of 2.31 GPa | ASTM D790 |
Resistencia a la flexión | 80.0 MPa Show Supplier Material materials with Resistencia a la flexión of 80.0 MPa | ASTM D790 |
Aplicaciones térmicas
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 83.0 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 83.0 °C | 1.8 MPa | ASTM D648 | ||
Inflamabilidad | UL94 HB |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 21.0 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 21.0 g/10min | ASTM D1238, 220°C,10kg/cm2 |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic appliances, Air conditioner, Panel, Humidifier water tank |