General
Property | Value | Comment |
---|---|---|
Densidad | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 65.0 [-] Show Supplier Material materials with Dureza Shore A of 65.0 [-] | ASTM D2240 |
Elongación | 800.0 % Show Supplier Material materials with Elongación of 800.0 % | ASTM D412 |
Resistencia a desgarros | 42.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 42.0 kN/m | ASTM D624 |
Resistencia a la tracción | 15.0 MPa Show Supplier Material materials with Resistencia a la tracción of 15.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Synthetic Leather, Furniture, Sports and Recreations. |