General
Property | Value | Comment |
---|---|---|
Bio-based content | 46.0 % Show Supplier Material materials with Bio-based content of 46.0 % | |
Densidad | 1.21 g/cm³ Show Supplier Material materials with Densidad of 1.21 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 75.0 [-] Show Supplier Material materials with Dureza Shore A of 75.0 [-] | ASTM D2240 |
Elongación | 1100.0 % Show Supplier Material materials with Elongación of 1100.0 % | ASTM D412 |
Resistencia a desgarros | 100.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 100.0 kN/m | ASTM D624 |
Resistencia a la tracción | 15.0 MPa Show Supplier Material materials with Resistencia a la tracción of 15.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging Material, Footwear, Consumer Goods, Automotive |