General
Property | Value | Comment |
---|---|---|
Bio-based content | 32.0 % Show Supplier Material materials with Bio-based content of 32.0 % | |
Densidad | 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.22 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 95.0 [-] Show Supplier Material materials with Dureza Shore A of 95.0 [-] | ASTM D2240 |
Elongación | 700.0 % Show Supplier Material materials with Elongación of 700.0 % | ASTM D412 |
Resistencia a desgarros | 195.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 195.0 kN/m | ASTM D624 |
Resistencia a la tracción | 44.0 MPa Show Supplier Material materials with Resistencia a la tracción of 44.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging Material, Footwear, Consumer Goods, Automotive |