General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.96 g/cm³ Show Supplier Material materials with Densidad of 0.96 g/cm³ | ASTM D793 |
Moisture absorption | 23.0 °C | 4.3E-3 % Show Supplier Material materials with Moisture absorption of 4.3E-3 % | ASTM D6982, 100°C - 1hr |
Mecánica
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 37 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 37 g/10min | ASTM D1238, 190°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Application areas | Irrigation Hoses, Electric Hoses - Film Grade | |
Color | Milky |