Property | Value |
---|---|
Recycled Content | 40 % Show Supplier Material materials with Recycled Content of 40 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 4 - 6 % Show Supplier Material materials with Elongación of 4 - 6 % | |
Flexural yield strength | 23.0 °C | 125 - 140 MPa Show Supplier Material materials with Flexural yield strength of 125 - 140 MPa | ISO 178 |
Límite elástico | 23.0 °C | 80 - 95 MPa Show Supplier Material materials with Límite elástico of 80 - 95 MPa | |
Módulo de flexión | 23.0 °C | 6.44 - 7.56 GPa Show Supplier Material materials with Módulo de flexión of 6.44 - 7.56 GPa | |
Módulo elástico | 23.0 °C | 6.9 - 8.1 GPa Show Supplier Material materials with Módulo elástico of 6.9 - 8.1 GPa | ISO 527-1,-2 |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 35 - 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 - 45 kJ/m² | ISO 179 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 3 - 6 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3 - 6 g/10min | 230°C/2.16kg, ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, household appliances, furniture, construction, fitting, industrial injection. Design of products tailored to customer requirements. | |
Color | Natural, Black | |
Fillers | 37-43% Glass Fiber |