General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.16 - 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.16 - 1.2 g/cm³ | ISO 1183-1, A |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo de flexión | 23.0 °C | 3.6 - 4.4 GPa Show Supplier Material materials with Módulo de flexión of 3.6 - 4.4 GPa | ISO 178 |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 25 - 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 25 - 35 kJ/m² | ISO 179 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 9 - 14 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 9 - 14 g/10min | 230°C/2.16kg, ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Injection Moulding | |
Color | Natural | |
Fillers | 37-43% Ultrafine Talc |