General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | max., ISO 787/2 |
Densidad | 23.0 °C | 0.94 - 0.96 g/cm³ Show Supplier Material materials with Densidad of 0.94 - 0.96 g/cm³ | ISO 1183 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Contenido de cenizas | 23.0 °C | 3 % Show Supplier Material materials with Contenido de cenizas of 3 % | max., ISO 3451-1, A |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo del volumen derretido | 0.2 - 0.4 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 0.2 - 0.4 cm³/10min | 190°C/2.16kg, ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Films and sheets (industrial, construction, ...) Bags and sacks Irrigation pipe, corrugated, wiring, multilayer Injection applications Asphalt sheet. Agricultural utensils, etc. | |
Color | Black |