General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.9 g/cm³ Show Supplier Material materials with Densidad of 1.9 g/cm³ | ASTM D792, ISO 1183 |
Mecánica
Property | Value | Testing Standard |
---|---|---|
Dureza Shore A | 88 [-] Show Supplier Material materials with Dureza Shore A of 88 [-] | ASTM D2240, ISO 868 |
92 [-] Show Supplier Material materials with Dureza Shore A of 92 [-] | ASTM D2240, ISO 868 | |
Módulo de flexión | 0.110 GPa Show Supplier Material materials with Módulo de flexión of 0.110 GPa | ASTM D790 |
Resistencia a desgarros | 17.5 kN/m Show Supplier Material materials with Resistencia a desgarros of 17.5 kN/m | ASTM D624 |
Resistencia a la tracción | 2.76 MPa Show Supplier Material materials with Resistencia a la tracción of 2.76 MPa | ASTM D638, ISO 527-2 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo de la masa derretida | 1.8 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 1.8 g/10min | ASTM D1238, ISO 1183 | 190°C/2.16kg |