General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 1.6 g/cm³ Show Supplier Material materials with Densidad of 1.6 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.25 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.25 [-] |
Elongación | 23.0 °C | 1.7 % Show Supplier Material materials with Elongación of 1.7 % |
Módulo elástico | 23.0 °C | 240 GPa Show Supplier Material materials with Módulo elástico of 240 GPa |
Resistencia a la tracción | 23.0 °C | 3400 MPa Show Supplier Material materials with Resistencia a la tracción of 3400 MPa |
Resistencia al cizallamiento | 23.0 °C | 40 MPa Show Supplier Material materials with Resistencia al cizallamiento of 40 MPa |
Technological properties
Property | ||
---|---|---|
Fillers | 68% Carbon Fiber | |
Processing methods | The production process is formed by laminating hot-pressed carbon fiber prepreg. |