General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Densidad of 8.3 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Available size round products (mm): 1-20 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 90 [-] Show Supplier Material materials with Dureza Brinell of 90 [-] |
Dureza Rockwell C | 23.0 °C | 0 [-] Show Supplier Material materials with Dureza Rockwell C of 0 [-] |
Dureza Vickers | 23.0 °C | 100 [-] Show Supplier Material materials with Dureza Vickers of 100 [-] |
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % |
Límite elástico | 23.0 °C | 240 MPa Show Supplier Material materials with Límite elástico of 240 MPa |
Módulo elástico | 23.0 °C | 115 GPa Show Supplier Material materials with Módulo elástico of 115 GPa |
Resistencia a la tracción | 23.0 °C | 290 MPa Show Supplier Material materials with Resistencia a la tracción of 290 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 380 W/(m·K) Show Supplier Material materials with Conductividad térmica of 380 W/(m·K) | for 20-200°C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 4.90E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 4.90E+7 S/m |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Electrical and electronic contacts, screws, for high performance relaxation | |
Corrosion properties | Corrosion resistance rating: 3 out of 5 | |
General machinability | Machinability: 60 % | |
Processing history | Condition: H12 |