General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.6 g/cm³ Show Supplier Material materials with Densidad of 7.6 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Available size round products (mm): from 16 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 190 [-] Show Supplier Material materials with Dureza Brinell of 190 [-] |
Dureza Rockwell C | 23.0 °C | 12 [-] Show Supplier Material materials with Dureza Rockwell C of 12 [-] |
Dureza Vickers | 23.0 °C | 186 [-] Show Supplier Material materials with Dureza Vickers of 186 [-] |
Elongación | 23.0 °C | 12 - 15 % Show Supplier Material materials with Elongación of 12 - 15 % |
Límite elástico | 23.0 °C | 320 - 400 MPa Show Supplier Material materials with Límite elástico of 320 - 400 MPa |
Módulo elástico | 23.0 °C | 125 GPa Show Supplier Material materials with Módulo elástico of 125 GPa |
Resistencia a la tracción | 23.0 °C | 650 - 700 MPa Show Supplier Material materials with Resistencia a la tracción of 650 - 700 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 40 W/(m·K) Show Supplier Material materials with Conductividad térmica of 40 W/(m·K) | for 20-200°C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 5.00E+6 S/m |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.5 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1.5 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Aerospace industry: rings, bushings and bearings for landing gears; Marine industry: distributor bodies, screws, forged parts | |
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
Friction | Friction behavior rating: 4 out of 5 | |
General machinability | Machinability: 40 % |