General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.8 g/cm³ Show Supplier Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Available size round products (mm): 1-14 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 290 - 314 [-] Show Supplier Material materials with Dureza Brinell of 290 - 314 [-] |
Dureza Rockwell C | 23.0 °C | 31 - 34 [-] Show Supplier Material materials with Dureza Rockwell C of 31 - 34 [-] |
Dureza Vickers | 23.0 °C | 300 - 330 [-] Show Supplier Material materials with Dureza Vickers of 300 - 330 [-] |
Elongación | 23.0 °C | 11 % Show Supplier Material materials with Elongación of 11 % |
Límite elástico | 23.0 °C | 910 - 1000 MPa Show Supplier Material materials with Límite elástico of 910 - 1000 MPa |
Módulo elástico | 23.0 °C | 115 GPa Show Supplier Material materials with Módulo elástico of 115 GPa |
Resistencia a la tracción | 23.0 °C | 950 - 1100 MPa Show Supplier Material materials with Resistencia a la tracción of 950 - 1100 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.72E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.72E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 55 W/(m·K) Show Supplier Material materials with Conductividad térmica of 55 W/(m·K) | for 20-200°C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 8.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 8.00E+6 S/m |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Connectors, precision mechanical & electrical parts | |
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
General machinability | Machinability: 60 % | |
Processing history | Condition: THX |