General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.6 g/cm³ Show Supplier Material materials with Densidad of 8.6 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 225 [-] Show Supplier Material materials with Dureza Brinell of 225 [-] |
Dureza Rockwell C | 23.0 °C | 20 [-] Show Supplier Material materials with Dureza Rockwell C of 20 [-] |
Dureza Vickers | 23.0 °C | 227 [-] Show Supplier Material materials with Dureza Vickers of 227 [-] |
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % |
Límite elástico | 23.0 °C | 590 - 690 MPa Show Supplier Material materials with Límite elástico of 590 - 690 MPa |
Módulo elástico | 23.0 °C | 145 GPa Show Supplier Material materials with Módulo elástico of 145 GPa |
Resistencia a la tracción | 23.0 °C | 780 - 830 MPa Show Supplier Material materials with Resistencia a la tracción of 780 - 830 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30 W/(m·K) | for 20-200°C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 5.00E+6 S/m |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.01 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1.01 [-] | max |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Parts for marine industry, aerospace industry and electrical industry | |
Corrosion properties | Corrosion resistance rating: 5 out of 5 | |
Friction | Friction behavior rating: 3 out of 5 | |
General machinability | Machinability: 30 % |