General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.5 g/cm³ Show Supplier Material materials with Densidad of 7.5 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 185 [-] Show Supplier Material materials with Dureza Brinell of 185 [-] |
Dureza Rockwell C | 23.0 °C | 12 [-] Show Supplier Material materials with Dureza Rockwell C of 12 [-] |
Dureza Vickers | 23.0 °C | 185 [-] Show Supplier Material materials with Dureza Vickers of 185 [-] |
Elongación | 23.0 °C | 8 % Show Supplier Material materials with Elongación of 8 % |
Límite elástico | 23.0 °C | 390 MPa Show Supplier Material materials with Límite elástico of 390 MPa |
Módulo elástico | 23.0 °C | 125 GPa Show Supplier Material materials with Módulo elástico of 125 GPa |
Resistencia a la tracción | 23.0 °C | 740 MPa Show Supplier Material materials with Resistencia a la tracción of 740 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 40 W/(m·K) Show Supplier Material materials with Conductividad térmica of 40 W/(m·K) | for 20-200°C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 5.00E+6 S/m |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.5 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1.5 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace industry: rings, bushings and bearings for landing gears, mechanical parts; Hydraulic industry: pump blocks | |
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
Friction | Friction behavior rating: 4 out of 5 | |
General machinability | Machinability: 40 % |