General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.6 g/cm³ Show Supplier Material materials with Densidad of 8.6 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 150 [-] Show Supplier Material materials with Dureza Brinell of 150 [-] |
Dureza Rockwell C | 23.0 °C | 0 [-] Show Supplier Material materials with Dureza Rockwell C of 0 [-] |
Dureza Vickers | 23.0 °C | 149 [-] Show Supplier Material materials with Dureza Vickers of 149 [-] |
Elongación | 23.0 °C | 12 % Show Supplier Material materials with Elongación of 12 % |
Límite elástico | 23.0 °C | 340 MPa Show Supplier Material materials with Límite elástico of 340 MPa |
Módulo elástico | 23.0 °C | 110 GPa Show Supplier Material materials with Módulo elástico of 110 GPa |
Resistencia a la tracción | 23.0 °C | 540 MPa Show Supplier Material materials with Resistencia a la tracción of 540 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30 W/(m·K) | for 20-200°C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 5.00E+6 S/m |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Bearing cages, rotor bars for engines, valve guides | |
Corrosion properties | Corrosion resistance rating: 3 out of 5 | |
Friction | Friction behavior rating: 5 out of 5 | |
General machinability | Machinability: 30 % | |
Processing history | Condition: H |