General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Densidad of 8.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 149 - 212 [-] Show Supplier Material materials with Dureza Brinell of 149 - 212 [-] |
Dureza Rockwell C | 23.0 °C | 0 - 18 [-] Show Supplier Material materials with Dureza Rockwell C of 0 - 18 [-] |
Dureza Vickers | 23.0 °C | 150 - 220 [-] Show Supplier Material materials with Dureza Vickers of 150 - 220 [-] |
Elongación | 23.0 °C | 10 - 15 % Show Supplier Material materials with Elongación of 10 - 15 % |
Límite elástico | 23.0 °C | 300 - 670 MPa Show Supplier Material materials with Límite elástico of 300 - 670 MPa |
Módulo elástico | 23.0 °C | 100 GPa Show Supplier Material materials with Módulo elástico of 100 GPa |
Resistencia a la tracción | 23.0 °C | 600 - 750 MPa Show Supplier Material materials with Resistencia a la tracción of 600 - 750 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Conductividad térmica of 35 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 5.00E+6 S/m |
Specific Electrical conductivity | 8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Plomo | 0.09 % Show Supplier Material materials with Plomo of 0.09 % | max. |