General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.65 g/cm³ Show Supplier Material materials with Densidad of 8.65 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 80 - 199 [-] Show Supplier Material materials with Dureza Brinell of 80 - 199 [-] |
Dureza Rockwell C | 23.0 °C | 0 - 15 [-] Show Supplier Material materials with Dureza Rockwell C of 0 - 15 [-] |
Dureza Vickers | 23.0 °C | 90 - 200 [-] Show Supplier Material materials with Dureza Vickers of 90 - 200 [-] |
Elongación | 23.0 °C | 2 - 40 % Show Supplier Material materials with Elongación of 2 - 40 % |
Límite elástico | 23.0 °C | 140 - 550 MPa Show Supplier Material materials with Límite elástico of 140 - 550 MPa |
Módulo elástico | 23.0 °C | 120 GPa Show Supplier Material materials with Módulo elástico of 120 GPa |
Resistencia a la tracción | 23.0 °C | 400 - 650 MPa Show Supplier Material materials with Resistencia a la tracción of 400 - 650 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Conductividad térmica of 35 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 5.00E+6 S/m |
Specific Electrical conductivity | 8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | ball point pen tips | |
General machinability | 85 % |