General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 104 - 216 [-] Show Supplier Material materials with Dureza Brinell of 104 - 216 [-] |
Dureza Rockwell C | 23.0 °C | 1 - 19 [-] Show Supplier Material materials with Dureza Rockwell C of 1 - 19 [-] |
Dureza Vickers | 23.0 °C | 111 - 175 [-] Show Supplier Material materials with Dureza Vickers of 111 - 175 [-] |
Elongación | 23.0 °C | 3 - 38 % Show Supplier Material materials with Elongación of 3 - 38 % |
Límite elástico | 23.0 °C | 241 - 700 MPa Show Supplier Material materials with Límite elástico of 241 - 700 MPa |
Módulo elástico | 23.0 °C | 115 GPa Show Supplier Material materials with Módulo elástico of 115 GPa |
Resistencia a la tracción | 23.0 °C | 491 - 780 MPa Show Supplier Material materials with Resistencia a la tracción of 491 - 780 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 33 W/(m·K) Show Supplier Material materials with Conductividad térmica of 33 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 4.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 4.00E+6 S/m |
Specific Electrical conductivity | 7 % IACS Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | ball point pen tips cold formed and machined eyeglass components screws | |
General machinability | 90 % |