General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Densidad of 8.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 80 - 103 [-] Show Supplier Material materials with Dureza Brinell of 80 - 103 [-] |
Dureza Vickers | 23.0 °C | 90 - 110 [-] Show Supplier Material materials with Dureza Vickers of 90 - 110 [-] |
Elongación | 23.0 °C | 1 - 30 % Show Supplier Material materials with Elongación of 1 - 30 % |
Límite elástico | 23.0 °C | 250 - 720 MPa Show Supplier Material materials with Límite elástico of 250 - 720 MPa |
Módulo elástico | 23.0 °C | 120 GPa Show Supplier Material materials with Módulo elástico of 120 GPa |
Resistencia a la tracción | 23.0 °C | 450 - 850 MPa Show Supplier Material materials with Resistencia a la tracción of 450 - 850 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 3.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 3.00E+6 S/m |
Specific Electrical conductivity | 5 % IACS Show Supplier Material materials with Specific Electrical conductivity of 5 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | writing instruments components for fiber optic connectors components for high safety locks spare parts for eyeglasses | |
General machinability | 90 % |