General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Densidad of 8.9 g/cm³ |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 23 W/(m·K) Show Supplier Material materials with Conductividad térmica of 23 W/(m·K) |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de temperatura de la resistencia | -20.0 °C | -8E-5 1/K Show Supplier Material materials with Coeficiente de temperatura de la resistencia of -8E-5 1/K | between -20 and +150°C |
150.0 °C | 4E-5 1/K Show Supplier Material materials with Coeficiente de temperatura de la resistencia of 4E-5 1/K | between -20 and +150°C | |
Resistividad eléctrica | 23.0 °C | 4.9E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 4.9E-7 Ω·m | |
Themo EMF | 23.0 °C | -4E-5 V/K Show Supplier Material materials with Themo EMF of -4E-5 V/K | against copper |
Technological properties
Property | ||
---|---|---|
Application areas | Resistors - Electrical shunts - Heating elements - Thermocouples |