General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 314 - 341 [-] Show Supplier Material materials with Dureza Brinell of 314 - 341 [-] |
Dureza Rockwell C | 23.0 °C | 34 - 37 [-] Show Supplier Material materials with Dureza Rockwell C of 34 - 37 [-] |
Dureza Vickers | 23.0 °C | 320 - 360 [-] Show Supplier Material materials with Dureza Vickers of 320 - 360 [-] |
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % |
Límite elástico | 23.0 °C | 900 MPa Show Supplier Material materials with Límite elástico of 900 MPa |
Módulo elástico | 23.0 °C | 120 GPa Show Supplier Material materials with Módulo elástico of 120 GPa |
Resistencia a la tracción | 23.0 °C | 1000 - 1100 MPa Show Supplier Material materials with Resistencia a la tracción of 1000 - 1100 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 52 W/(m·K) Show Supplier Material materials with Conductividad térmica of 52 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 8.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 8.00E+6 S/m |
Specific Electrical conductivity | 14 % IACS Show Supplier Material materials with Specific Electrical conductivity of 14 % IACS |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.01 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1.01 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Niclafor can be a substitute to Copper-Titanium and Copper-Beryllium for some applications. It used in the automotive industry, for example on bushings and bearings, eg. small end rings in high performance car engines. Niclafor® is also a material of reference in the eyewear industry: its high elasticity and formability allow light and durable designs. Niclafor® is extensively used in the electronics industry, including aerospace systems, for applications such as EMI shielding and connector parts. Summary of typical applications: Electronics (Relays, EMI Shielding, etc.), Connectors, Electrical engineering, Automotive, Telecom and Mobile phones, Eyewear and Spectacles industry, Domestic appliance. |