General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.76 g/cm³ Show Supplier Material materials with Densidad of 8.76 g/cm³ |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | for 20-200°C |
Conductividad térmica | 23.0 °C | 22 W/(m·K) Show Supplier Material materials with Conductividad térmica of 22 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 4.2E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 4.2E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Precision resistors / Electrical shunts in electricity meters / Electrical shunts in DC ammeters |