General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | ASTM D297 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 500 % Show Supplier Material materials with Elongación of 500 % | ASTM D412 | ||
Resistencia a la tracción | 23.0 °C | 20 MPa Show Supplier Material materials with Resistencia a la tracción of 20 MPa | ASTM D412 | ||
Impact strength, Izod notched, ASTM | No Break | ||||
Impact strength, Izod unnotched, ASTM | No Break |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | V-0 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 6.3 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 6.3 [-] | ASTM D150 |
Dissipation factor, 1MHz | 23.0 °C | 0.1 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.1 [-] | ASTM D150 |
Rigidez dieléctrica | 23.0 °C | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | ASTM D149 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & Cable applications | |
Processing methods | Injection Molding, Extrusion |