General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.22 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 60 [-] Show Supplier Material materials with Dureza Shore D of 60 [-] | ASTM D2240 |
Elongación | 23.0 °C | 400 % Show Supplier Material materials with Elongación of 400 % | ASTM D412 |
Resistencia a desgarros | 23.0 °C | 160 kN/m Show Supplier Material materials with Resistencia a desgarros of 160 kN/m | ASTM D624 |
Resistencia a la flexión | 23.0 °C | 300 MPa Show Supplier Material materials with Resistencia a la flexión of 300 MPa | |
Resistencia a la tracción | 23.0 °C | 25 MPa Show Supplier Material materials with Resistencia a la tracción of 25 MPa | ASTM D412 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Brittleness temperature | -50 °C Show Supplier Material materials with Brittleness temperature of -50 °C | D746 |
Temperatura de fusión | 210 °C Show Supplier Material materials with Temperatura de fusión of 210 °C | |
Temperatura de reblandecimiento Vicat | 190 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 190 °C |
Technological properties
Property | ||
---|---|---|
Processing methods | Pre-drying: 100°C for 4-8 hr, Injection temperature: 10-20°C higher than melting temperature, Extrusion and blow temperature: higher than melting temperature |