General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 80 [-] Show Supplier Material materials with Dureza Shore A of 80 [-] | ASTM D2240 |
Elongación | 23.0 °C | 390 % Show Supplier Material materials with Elongación of 390 % | ASTM D412 |
Resistencia a desgarros | 23.0 °C | 38 kN/m Show Supplier Material materials with Resistencia a desgarros of 38 kN/m | ASTM D624 |
Resistencia a la tracción | 23.0 °C | 11.7 MPa Show Supplier Material materials with Resistencia a la tracción of 11.7 MPa | ASTM D412 |
Set de compresión | 70.0 °C | 64 [-] Show Supplier Material materials with Set de compresión of 64 [-] | ASTM D395 |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Processing methods | Pre-drying: 60°C for 6-8 hr, Extrusion: Hopper Temperature: 130-140°C, Middle Temperature: 140-150°C, Measurment Temperature: 140-150°C, Front Temperature: 150-170°C, Mold Temperature: 150-170°C, Melt Temperature: 160°C, Comp. Ratio: 2.5:1, Screen: 20-60 Mesh - Injection: Rear Temperature: 130-140°C, Middle Temperature: 140-160°C, Front Temperature: 160-190°C, Nozzle Temperature: 170-190°C, Melt Temperature:170°C, Mold Temperature: 30-80°C, Speed: 100-200rpm, Back Pressure 0.05-05 Mpa |