General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 85 [-] Show Supplier Material materials with Dureza Shore A of 85 [-] | ASTM D2240 |
Elongación | 23.0 °C | 620 % Show Supplier Material materials with Elongación of 620 % | ASTM D412 |
Resistencia a la tracción | 23.0 °C | 20 MPa Show Supplier Material materials with Resistencia a la tracción of 20 MPa | ASTM D412 |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL-1581 VW-1 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 5.4 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 5.4 [-] | ASTM D150 |
Dissipation factor, 1MHz | 23.0 °C | 0.05 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.05 [-] | ASTM D150 |
Rigidez dieléctrica | 23.0 °C | 18 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 18 kV/mm | ASTM D149 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Processing methods | Pre-drying: 80°C for 4-8 hr, Injection temperature: 170-190°C, Extrusion temperature: 170-180°C, Injection pressure: 40-60MPa, Filter: 100-200 mesh |