General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 70 [-] Show Supplier Material materials with Dureza Shore A of 70 [-] | ASTM D2240 |
Elongación | 23.0 °C | 500 % Show Supplier Material materials with Elongación of 500 % | ASTM D412 |
Resistencia a la tracción | 23.0 °C | 7 MPa Show Supplier Material materials with Resistencia a la tracción of 7 MPa | ASTM D412 |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL94 V-0 (3mm) |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | min., ASTM D149 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & Cable applications | |
Processing methods | Hopper Temperature: 150-170°C, Transmission Temperature: 180-200°C, Measurement Temperature: 200-230°C, Die Temperature: 190-220°C |